EN ISO 12947-2 |
31787-01 |
Dec 11, 2006 |
English |
ASTM D4966 Martindale |
2-67210-6 |
Apr 18, 2007 |
English |
BS EN ISO 105 B02 Method 2 |
31787-01 |
Dec 11, 2006 |
English |
BS EN ISO 105 B02 Method 2 |
33310 |
Aug 10, 2007 |
English |
AATCC 16 Lightfastness/ACT 40HRS |
2-67211-1 |
Apr 17, 2007 |
English |
BS EN ISO 105-X12 |
31787-01 |
Dec 11, 2006 |
English |
BS EN 1021 1&2 35 kg/m3 CMHR foam |
31787 |
Dec 11, 2006 |
English |
Calif. Bull. 117E |
67210-0 |
Apr 18, 2007 |
English |
BS 5852 Part 1 0,1 Cigarette & match 50 kg/m3 CMHR foam |
R13327 |
Aug 7, 2008 |
English |
Will also pass other flammability standards. Flame retardant performance is dependent upon the foam used and fireproof treatment. |
- |
Mar 15, 2012 |
|
BS 5852 Part 1 Cigarette & match 20-22 kg/m3 non-fire retardant polyurethane foam |
49155-01 |
Jan 12, 2012 |
English |
BS 5852 Part 1 0,1 Cigarette & match 20-22 kg/m3 non-fire retardant polyurethane foam |
49155-01 |
Jan 12, 2012 |
English |
BS EN ISO 12945-2 |
32364 |
Feb 20, 2007 |
English |
ASTM D 3511/ACT Pilling |
2-67210-3 |
Apr 12, 2007 |
English |
BS EN ISO 6330 P7A Drying PC: Flat Dry 40 degree |
31787-01 |
Dec 11, 2006 |
English |
AATCC 8 or 116 wet/dry crocking ACT-2001 |
2-67211-0 |
Apr 13, 2007 |
English |
|
|
|
|